TPEE/美國(guó)杜邦/G3548L 硬度35D 進(jìn)口tpee塑料
原料技術(shù)數(shù)據(jù)
性能項(xiàng)目 | 試驗(yàn)條件[狀態(tài)] | 測(cè)試方法 | 測(cè)試數(shù)據(jù) | 數(shù)據(jù)單位 | ||
基本性能 | 24小時(shí)吸水率 | ASTM D-570 | 5 | % | ||
物理性能 | 熔體流動(dòng)速率 | ASTM D-1238 | 10 | g/10min | ||
泰伯磨耗量 | H 18輪 | ASTM D-1044 | 310 | mg/1000rev | ||
泰伯磨耗量 | CS-17輪 | ASTM D-1044 | 30 | mg/1000rev | ||
比重 | ASTM D-792 | 1.15 | ||||
機(jī)械性能 | 斷裂伸長(zhǎng) | ASTM D-638 | 200 | % | ||
硬度計(jì)硬度 | ASTM D-2240 | 35 | ||||
斷裂拉伸力 | ASTM D-638 | 10.3 | Mpa | |||
初耐撕裂性能 | ASTM D-1004 | 51 | kn/m | |||
揉曲模量 | 23℃ | ASTM D-790 | 32.4 | Mpa | ||
拉伸力 | 5%伸長(zhǎng) | ASTM D-638 | 1.7 | Mpa | ||
10%伸長(zhǎng) | ASTM D-638 | 2.6 | Mpa | |||
埃佐沖擊強(qiáng)度 | 23℃ | ASTM D-256 | 不破裂 | J/m | ||
熱性能 | 維卡軟化點(diǎn) | ASTM D-1525 | 77 | ℃ | ||
熔點(diǎn) | ASTM D-3418 | 156 | ℃ | |||
熱畸變溫度 | @0.5Mpa | ASTM D-648 | N/A | ℃ | ||
熱畸變溫度 | @0.18Mpa | ASTM D-648 | N/A | ℃ | ||
其它性能 | 耐揉曲切口增長(zhǎng)性能 | ASTM D-1052 | >1×106 |